New

Ask Wove anything about tariffs.

Try Tariff Assistant

Defective Superalloy Billets from Mexico

Inconel 718 billets with centerline piping from scrap VIM without ESR remelt. Turbine disk production requires secondary remelting per HTS 9817.00.90.40.

Duty Rate — Mexico → United States

10%

Rate breakdown

9903.05.5510%Except for products described in headings 9903.05.85–9903.05.92 and 9903.05.94, articles the product of Mexico, as provided for in U.S. note 52 to this subchapter

Import Tips

• VIM process records and macroetch photos of centerline defects,Chemical analysis matching scrap composition without adjustments,Usable superalloy billets under alloy-specific Chapter 72/81 codes

Defective Superalloy Billets from Mexico — Import Duty Rate | HTS 9817.00.90.40