Argon Oxygen Decarburized Ferronickel from Germany
AOD-process ferronickel refined to ultra-low carbon (<0.03%) using argon-oxygen decarburization for duplex stainless production. Contains 25-30% nickel with controlled impurities. Classifies under HTS 7202.60.00.00 as refined ferronickel alloy.
Duty Rate — Germany → United States
0%
Rate breakdown
9903.03.030%Articles the product of any country, as provided for in subdivision (aa)(ii) of U.S. note 2 to this subchapter
Import Tips
• AOD certification and melt logs essential to prove decarburization process applied
• Higher value product; ensure insurance covers premium pricing during ocean transit