Argon Oxygen Decarburized Ferronickel

AOD-process ferronickel refined to ultra-low carbon (<0.03%) using argon-oxygen decarburization for duplex stainless production. Contains 25-30% nickel with controlled impurities. Classifies under HTS 7202.60.00.00 as refined ferronickel alloy.

Import Duty Rates by Country of Origin

Origin CountryMFN RateCh.99 SurchargesTotal Effective Rate
๐Ÿ‡จ๐Ÿ‡ณChinaFree+25.0%25%
๐Ÿ‡ฒ๐Ÿ‡ฝMexicoFreeโ€”Free
๐Ÿ‡จ๐Ÿ‡ฆCanadaFreeโ€”Free
๐Ÿ‡ฉ๐Ÿ‡ชGermanyFreeโ€”Free
๐Ÿ‡ฏ๐Ÿ‡ตJapanFreeโ€”Free

Alternative Classifications

This product could be classified differently depending on its characteristics or intended use.

7223.00.10Higher: 35% vs 25%

If melted and cast into ingots for wire rod

Post-melting into steel products shifts to Chapter 72 semifinished articles.

7506.20Lower: 12.5% vs 25%

If further alloyed into nickel plate

Plates/sheets of nickel alloys classify in Chapter 75 worked forms.

Not sure which classification is right?

Our AI classifier can analyze your specific product and recommend the correct HTS code with confidence.

Import Tips & Compliance

โ€ข AOD certification and melt logs essential to prove decarburization process applied

โ€ข Higher value product; ensure insurance covers premium pricing during ocean transit

โ€ข Test for tramp elements (Cu, Sn) as AOD doesn't remove all impurities