Bleached Mechanical Pulp (BMP) Aspen from China

BMP from hardwood undergoes mechanical pulping followed by peroxide bleaching for whiteness in hygiene papers without full chemical delignification. Yield remains high (90%+). Still mechanical woodpulp per HTS 4701.00.00.00 as bleaching doesn't change process classification.

Duty Rate — China → United States

37.5%

Rate breakdown

9903.88.0325%Except as provided in headings 9903.88.13, 9903.88.18, 9903.88.33, 9903.88.34, 9903.88.35, 9903.88.36, 9903.88.37, 9903.88.38, 9903.88.40, 9903.88.41, 9903.88.43, 9903.88.45, 9903.88.46, 9903.88.48, 9903.88.56, 9903.88.64, 9903.88.66, 9903.88.67, 9903.88.68, or 9903.88.69, articles the product of China, as provided for in U.S. note 20(e) to this subchapter and as provided for in the subheadings enumerated in U.S. note 20(f)
9903.05.3112.5%Section 301 (forced labor) — additional 12.5% ad valorem on products of China

Import Tips

Specify bleaching agent (hydrogen peroxide only) to differentiate from chemical pulp bleaches like chlorine

Lab reports showing post-bleach lignin >15% confirm mechanical status

Avoid 'fully bleached' terminology that suggests chemical grades