Rene 41 Nickel-Based Superalloy Wire

Rene 41 superalloy wire is used for turbine blades and hot-section components, offering exceptional creep resistance above 1800Β°F. In a not cold-formed condition, this nickel-based superalloy wire is classified under tariff item 7505.22.00 as nickel alloy wire.

Import Duty Rates by Country of Origin

Origin CountryMFN TariffSurtaxesTotal Effective Rate
πŸ‡¨πŸ‡³ChinaFreeβ€”Free
πŸ‡²πŸ‡½MexicoFreeβ€”Free
πŸ‡ΊπŸ‡ΈUnited StatesFreeβ€”Free
πŸ‡©πŸ‡ͺGermanyFreeβ€”Free
πŸ‡―πŸ‡΅JapanFreeβ€”Free

More Specific Codes

This product may fall under a more specific subheading:

Alternative Classifications

This product could be classified differently depending on its characteristics or intended use.

7505.21.00Same rate: Free

If the wire is cold-formed during production

Cold-formed nickel alloy wire is classified under 7505.21.

7504.00.00Same rate: Free

If the product is in powder form for additive manufacturing

Nickel alloy powders are classified under heading 7504.

8108.90.00Same rate: Free

If the wire is actually a titanium alloy, not nickel-based

Titanium alloy wire is classified under Chapter 81.

Not sure which classification is right?

The Tariff Assistant works through the GRI rules on your specific product to reach the right tariff item β€” and can price the duty on it in the same conversation.

Import Tips & Compliance

β€’ Provide a full chemical analysis to demonstrate nickel predominance by weight over cobalt, chromium, and other elements

β€’ Verify the wire is not cold-formed to use 7505.22.00

β€’ For aerospace applications, ensure compliance with any Canadian import controls on dual-use goods

Related Products under Tariff item 7505.22.00

Alloy 20Cb-3 Nickel-Iron-Chromium Wire

Alloy 20Cb-3 (Carpenter 20) wire is a nickel-iron-chromium alloy with outstanding resistance to sulfuric acid and chloride stress corrosion, making it ideal for pharmaceutical and food processing equipment. As a wire of nickel alloy, it falls under tariff item 7505.22.00, which covers nickel alloy wire regardless of cold-working.

Alloy 20 Cold-Formed Welding Wire

Cold-formed welding wire made from Alloy 20, a nickel-iron-chromium alloy, offering superior resistance to sulfuric acid environments. The cold-forming process and nickel alloy composition place it under tariff item 7505.22.00 for wire of nickel alloys.

Constantan Nickel-Copper Wire

Constantan wire, a nickel-copper alloy with roughly 55% copper and 45% nickel, provides stable electrical resistance for precision thermocouples and strain gauges. Although copper is present in higher proportion, the product is classified as a nickel alloy because nickel predominates by weight over each other element, placing it under tariff item 7505.22.00.

Custom 718 Cold-Formed Profile Wire

Cold-formed shaped profile wire from Custom Age 718 (Inconel 718 variant) nickel alloy, used in turbine engine components. The cold-forming process and nickel alloy base classify it under tariff item 7505.22.00.

Hastelloy C-276 Cold-Formed Flat Wire

Flat profile cold-formed wire from Hastelloy C-276, a nickel-molybdenum-chromium alloy known for resistance to pitting and stress corrosion cracking. This cold-formed nickel alloy wire falls under tariff item 7505.22.00.

Hastelloy C-276 Nickel-Molybdenum Wire

Hastelloy C-276 wire is a nickel-molybdenum-chromium alloy offering superior resistance to pitting, crevice corrosion, and stress corrosion cracking in aggressive chemical environments. Used in pollution control and chemical processing, this wire is classified under tariff item 7505.22.00 as a nickel alloy wire that is not cold-formed.