Creep Testing Furnace Specimen Holder from Japan
High-temperature alloy specimen holder for creep testing machines, positioning metal samples under constant load at elevated temperatures (up to 1200°C). Accessory for long-term metal property testing under HTS 9024.90.00.40.
Duty Rate — Japan → United States
12.5%
Rate breakdown
9903.05.4912.5%Except for products described in headings 9903.05.85–9903.05.92, articles the product of Japan, with an ad valorem (or ad valorem equivalent) rate of duty under column 1 less than 12.5 percent, as provided for in U.S. note 52 to this subchapter
Import Tips
• Include material certs (e.g
• Inconel 718) and max temp rating in documentation
• Reference ASTM E139 creep standards for classification support