Chilled Iron Paper Roll from Japan

Chilled cast iron roll with hardened shell for wear resistance in pulp dryer sections and calenders. HTS 8420.91.20.00 designation reflects paper machine rolling function. Pearlitic matrix provides 500-600 HB hardness for abrasive furnish.

Duty Rate — Japan → United States

12.5%

Rate breakdown

9903.05.4912.5%Section 301 (forced labor) — Japan (col1 rate < 12.5 percent): MFN < 12.5% → total duty capped at 12.5%

Import Tips

Include Brinell hardness certification and microstructure analysis; document face length for paper width matching; verify no glass/textile features