Cast Iron Repair Welding Rod from China
Nickel-coated flux-cored rods for flame welding cracked cast iron engine blocks and machinery. High nickel for crack resistance. Under 8311.30.60.00 as other coated rods for welding.
Duty Rate — China → United States
35%
Rate breakdown
9903.03.0110%Except for products described in headings 9903.03.02–9903.03.11, articles the product of any country, as provided for in subdivision (aa) of U.S. note 2 to this subchapter
9903.88.0325%Except as provided in headings 9903.88.13, 9903.88.18, 9903.88.33, 9903.88.34, 9903.88.35, 9903.88.36, 9903.88.37, 9903.88.38, 9903.88.40, 9903.88.41, 9903.88.43, 9903.88.45, 9903.88.46, 9903.88.48, 9903.88.56, 9903.88.64, 9903.88.66, 9903.88.67, 9903.88.68, or 9903.88.69, articles the product of China, as provided for in U.S. note 20(e) to this subchapter and as provided for in the subheadings enumerated in U.S. note 20(f)
Import Tips
• Specify nickel-iron composition to avoid metal carbide confusion
• Include welding procedure specs (WPS) for validation