Rhenium Alloying Powder for Superalloys from China
Atomized rhenium powder used as master alloy addition in nickel-based superalloys for gas turbines. HTS 8112.41.50.00 applies to this unwrought powder form before melting and alloying. Enhances creep resistance at extreme temperatures.
Duty Rate — China → United States
28%
Rate breakdown
9903.88.0325%Except as provided in headings 9903.88.13, 9903.88.18, 9903.88.33, 9903.88.34, 9903.88.35, 9903.88.36, 9903.88.37, 9903.88.38, 9903.88.40, 9903.88.41, 9903.88.43, 9903.88.45, 9903.88.46, 9903.88.48, 9903.88.56, 9903.88.64, 9903.88.66, 9903.88.67, 9903.88.68, or 9903.88.69, articles the product of China, as provided for in U.S. note 20(e) to this subchapter and as provided for in the subheadings enumerated in U.S. note 20(f)
9903.05.860%Articles provided for in subdivision (b) of U.S. note 52 to this subchapter
Import Tips
• Specify 'for remelt only' on commercial invoice to avoid parts classification
• Batch test for tramp elements; high impurities shift to waste subheading
• Use nitrogen-purged containers; oxygen pickup common pitfall affecting purity declaration