Hafnium Foil for Superalloy Cladding from China

Thin hafnium foil sheets used to clad nickel superalloy turbine blades for oxidation resistance. HTS 8112.39.00.00 for 'other' hafnium sheet/foil beyond basic thicknesses.

Duty Rate — China → United States

41.5%

Rate breakdown

9903.05.3112.5%Except for products described in headings 9903.05.85–9903.05.92, articles the product of China, as provided for in U.S. note 52 to this subchapter
9903.88.0325%Except as provided in headings 9903.88.13, 9903.88.18, 9903.88.33, 9903.88.34, 9903.88.35, 9903.88.36, 9903.88.37, 9903.88.38, 9903.88.40, 9903.88.41, 9903.88.43, 9903.88.45, 9903.88.46, 9903.88.48, 9903.88.56, 9903.88.64, 9903.88.66, 9903.88.67, 9903.88.68, or 9903.88.69, articles the product of China, as provided for in U.S. note 20(e) to this subchapter and as provided for in the subheadings enumerated in U.S. note 20(f)

Import Tips

• Include thickness (<0.2mm typical) and surface finish specs in commercial invoices

• Protect from ambient oxidation during transit with inert atmosphere packaging

• Validate against AMS specifications for aerospace qualification traceability