Cobalt Master Alloy Ingots for Superalloys from Canada

Unwrought cobalt-based master alloy ingots (Co-Cr-W) used in turbine blade production, with cobalt as predominant metal. HTS 8105.20.60.00 applies as 'other' unwrought cobalt per Chapter 81 alloy note (cobalt >99% or > any other element). These are not pure cobalt but intermediate products of cobalt metallurgy.

Duty Rate — Canada → United States

0%

Rate breakdown

9903.05.860%Articles provided for in subdivision (b) of U.S. note 52 to this subchapter

Import Tips

• Submit detailed chemical analysis showing cobalt dominance to meet Chapter 81 alloy definitions

• Avoid common error of classifying as nickel alloys (8112) if cobalt content prevails

• Obtain end-use statements for aerospace buyers to support duty drawback claims