Molybdenum Powder for Superalloy Production
Coarse molybdenum powder used in vacuum arc remelting for nickel-based superalloys in turbine blades. Classified under HTS 8102.10.00.00 as base molybdenum powder per Chapter 81 hierarchy. 50-150 micron size optimized for melting practice.
Import Duty Rates by Country of Origin
Alternative Classifications
This product could be classified differently depending on its characteristics or intended use.
If master alloyed with nickel beforehand
Nickel alloy powders including Mo classified by predominant nickel content in Chapter 75.
If reduced to iron-molybdenum pre-alloy
Ferromolybdenum powders follow iron/steel alloy classification in Chapter 72.
If in bulk sintered form for alloying
Wrought or sintered molybdenum articles excluding powders in 8105.90.
Not sure which classification is right?
The Tariff Assistant works through the GRI rules on your specific product to reach the right HTS code — and can price the duty on it in the same conversation.
Import Tips & Compliance
• Provide alloy master melt certificates showing intended 3-5% Mo addition rates
• Hydrogen decrepitation process documentation proves powder vs wrought origin
• Avoid pre-alloyed Mo-Ni powder which classifies under 8112.99 for cobalt alloys
Related Products under HTS 8102.10.00.00
Molybdenum Powder for 3D Metal Printing
Fine molybdenum powder optimized for selective laser melting (SLM) in additive manufacturing of high-temperature parts. HTS 8102.10.00.00 applies as it's unwrought molybdenum powder with purity exceeding Chapter 81 alloy threshold. Typically 15-45 micron spherical particles.
Electrolytic Molybdenum Powder
Dendritic molybdenum powder produced by fused salt electrolysis, noted for high purity and green color. HTS 8102.10.00.00 specifically covers this production method's powder. Used primarily in lighting filament supports and electronics.
Molybdenum Powder for Sintered Parts
Press-and-sinter grade molybdenum powder for manufacturing heat sinks and electrical contacts. Uniform 5-20 micron size distribution ensures high green strength. HTS 8102.10.00.00 as unwrought powder per tariff structure.
Recycled Molybdenum Powder from Scrap
Secondary molybdenum powder produced from machined scrap recycling, suitable for lower purity applications. Still qualifies HTS 8102.10.00.00 as molybdenum powder >99% base metal content. Cost-effective for non-critical alloying.
Molybdenum Metal Powder 99.9% Pure
High-purity molybdenum powder with 99.9% molybdenum content, used in metallurgy and alloy production. Classified under HTS 8102.10.00.00 as it is molybdenum powder, explicitly covered in this subheading for powders of molybdenum. Particle size typically ranges from 1-10 microns for fine applications.
Atomized Molybdenum Powder for Thermal Spraying
Atomized molybdenum powder designed for plasma or HVOF thermal spray coatings on industrial components. Falls under HTS 8102.10.00.00 as pure molybdenum powder per Chapter 81 definitions (molybdenum >99% by weight). Spherical particles ensure high flowability and coating density.