Rene 41 Nickel-Based Superalloy Wire from Japan

Rene 41 superalloy wire for turbine blades and hot-section components offers exceptional creep resistance above 1800°F. Not cold-formed condition classifies under HTS 7505.22.50.00 as nickel alloy wire.

Duty Rate — Japan → United States

12.5%

Rate breakdown

9903.05.4912.5%Except for products described in headings 9903.05.85–9903.05.92, articles the product of Japan, with an ad valorem (or ad valorem equivalent) rate of duty under column 1 less than 12.5 percent, as provided for in U.S. note 52 to this subchapter

Import Tips

• ITAR/EAR export control documentation often required for superalloy wire

• Solution annealing certificates verify proper heat treatment condition

• Vacuum induction melt (VIM) process documentation confirms quality grade