Rene 41 Nickel-Based Superalloy Wire from China

Rene 41 superalloy wire for turbine blades and hot-section components offers exceptional creep resistance above 1800°F. Not cold-formed condition classifies under HTS 7505.22.50.00 as nickel alloy wire.

Duty Rate — China → United States

40.1%

Rate breakdown

9903.05.3112.5%Except for products described in headings 9903.05.85–9903.05.92, articles the product of China, as provided for in U.S. note 52 to this subchapter
9903.88.0325%Except as provided in headings 9903.88.13, 9903.88.18, 9903.88.33, 9903.88.34, 9903.88.35, 9903.88.36, 9903.88.37, 9903.88.38, 9903.88.40, 9903.88.41, 9903.88.43, 9903.88.45, 9903.88.46, 9903.88.48, 9903.88.56, 9903.88.64, 9903.88.66, 9903.88.67, 9903.88.68, or 9903.88.69, articles the product of China, as provided for in U.S. note 20(e) to this subchapter and as provided for in the subheadings enumerated in U.S. note 20(f)

Import Tips

• ITAR/EAR export control documentation often required for superalloy wire

• Solution annealing certificates verify proper heat treatment condition

• Vacuum induction melt (VIM) process documentation confirms quality grade