High Leaded Tin Bronze C93800 Ingot from China

C93800 high leaded tin bronze has 78% copper, 15% lead, 7% tin unwrought. HTS 7403.29.01 other copper alloys due to lead dominance preventing standard bronze. Bearings and bushings where lubrication needed.

Duty Rate — China → United States

26%

Rate breakdown

9903.88.0325%Except as provided in headings 9903.88.13, 9903.88.18, 9903.88.33, 9903.88.34, 9903.88.35, 9903.88.36, 9903.88.37, 9903.88.38, 9903.88.40, 9903.88.41, 9903.88.43, 9903.88.45, 9903.88.46, 9903.88.48, 9903.88.56, 9903.88.64, 9903.88.66, 9903.88.67, 9903.88.68, or 9903.88.69, articles the product of China, as provided for in U.S. note 20(e) to this subchapter and as provided for in the subheadings enumerated in U.S. note 20(f)
9903.03.030%Articles the product of any country, as provided for in subdivision (aa)(ii) of U.S. note 2 to this subchapter

Import Tips

RoHS exemption documentation for high lead content

Lead volatility during melting; fume extraction specs required

Free-machining grade; chip breakability affects end use declaration