Heat-Resisting 309 Stainless Bloom from Germany

Bloom of 309 heat-resisting stainless steel (<0.3% C, 22-24% Cr) for furnace parts per Chapter note (g). Classifies HTS 7218.99.00.90 as other semi-finished stainless. High-temperature oxidation resistance.

Duty Rate — Germany → United States

10%

Rate breakdown

9903.03.0110%Except for products described in headings 9903.03.02–9903.03.11, articles the product of any country, as provided for in subdivision (aa) of U.S. note 2 to this subchapter

Import Tips

Document low carbon (<0.3%) and Cr (4-10.5%) matching heat-resisting definition

No enameling/varnishing; treated as further worked

Test certs must exclude tool steel elements