White Pig Iron with High Phosphorus Content from Mexico

High-phosphorus (>0.5%) nonalloy pig iron designed for white cast iron production, cast in pig or block forms. HTS 7201.20.00.00 applies as it meets the nonalloy primary form criteria with excess phosphorus for hardness in castings. Used in applications requiring wear resistance.

Duty Rate — Mexico → United States

10%

Rate breakdown

9903.03.0110%Except for products described in headings 9903.03.02–9903.03.11, articles the product of any country, as provided for in subdivision (aa) of U.S. note 2 to this subchapter

Import Tips

Label shipments clearly as 'nonalloy pig iron >0.5% P' with supporting lab assays

Ensure no cladding or coatings; Chapter 72 defines 'further worked' to prevent misclassification