Polycrystalline Synthetic Diamond Powder 325 Mesh Lapping Grade from Japan
Polycrystalline synthetic diamond powder at 325 mesh (44 micron), optimized for lapping carbide and ceramic substrates. Classifies in 7105.10.0030 as it meets synthetic diamond powder definition with 80 mesh or finer particles per sieve note. Key for hard disk drive manufacturing.
Duty Rate — Japan → United States
10%
Rate breakdown
9903.03.0110%Except for products described in headings 9903.03.02–9903.03.11, articles the product of any country, as provided for in subdivision (aa) of U.S. note 2 to this subchapter
Import Tips
• Batch testing for friability index recommended; high friability may trigger abrasion testing by CBP
• Package in nitrogen-flushed containers; oxidation proof required for fines storage