</>Build with Tariff Intelligence|Programmatic access to tariff calculations and HS code classification.Explore Developer Resources →

PVC Suspension Resin K-67 from Japan

Suspension polymerized nonplasticized PVC resin with K-value 65-67, primary form for rigid pipe extrusion. Classified in 3904.21.00.00 due to pure vinyl chloride composition exceeding 95% monomer content.

Duty Rate — Japan → United States

12.5%

Rate breakdown

9903.05.4912.5%Section 301 (forced labor) — Japan (col1 rate < 12.5 percent): MFN < 12.5% → total duty capped at 12.5%

Import Tips

Submit polymerization process documentation confirming suspension method and no plasticizer addition

Label shipments with K-value range to match rigid applications and avoid soft grade confusion

Comply with REACH-like certifications for vinyl chloride monomer residuals