Steel Mill Spent Pickling Liquor from Japan
Hydrochloric acid waste from continuous steel pickling lines, containing high iron chloride concentrations. Under HTS 3825.50.00.00 as metal-pickling liquor waste, chapter note 6(d). Major source of ferrous chloride for water treatment.
Duty Rate — Japan → United States
12.5%
Rate breakdown
9903.05.4912.5%Section 301 (forced labor) — Japan (col1 rate < 12.5 percent): MFN < 12.5% → total duty capped at 12.5%
Import Tips
• Specify regeneration potential (HCl recovery) in documentation
• Monitor free acid vs metal salt content ratio