</>Build with Tariff Intelligence|Programmatic access to tariff calculations and HS code classification.Explore Developer Resources →

High-Strength Nonrefractory Concrete Mix from Japan

Dry powder concrete achieving 10,000 PSI strength with silica fume and superplasticizers for bridges and high-load structures. Nonrefractory for ambient conditions. Under HTS 3824.50.00 as advanced prepared nonrefractory concrete.

Duty Rate — Japan → United States

12.5%

Rate breakdown

9903.05.4912.5%Section 301 (forced labor) — Japan (col1 rate < 12.5 percent): MFN < 12.5% → total duty capped at 12.5%

Import Tips

Provide mix design reports for engineering approvals

Declare silica fume percentage for health/safety filings

Coordinate with DOT specs for infrastructure projects