WC-TiC-Co 80/15/5 Ready-to-Press Powder from Germany
80% WC, 15% TiC, 5% cobalt binder nonagglomerated powder specifically graded for press-and-sinter tooling. Under 3824.30.00.00 as mixed carbides with metallic binder not yet agglomerated. Standard for indexable inserts.