</>Build with Tariff Intelligence|Programmatic access to tariff calculations and HS code classification.Explore Developer Resources →

Nickel Laterite Leaching Ash with Arsenic from Japan

Ash from nickel laterite ore leaching processes containing arsenic and nickel compounds, for recovery in industry. Under HTS 2620.99.8500 as other residues with arsenic and metals.

Duty Rate — Japan → United States

12.5%

Rate breakdown

9903.05.4912.5%Section 301 (forced labor) — Japan (col1 rate < 12.5 percent): MFN < 12.5% → total duty capped at 12.5%

Import Tips

Declare intended use for chemical manufacture to meet heading criteria

Avoid common pitfall of incomplete origin docs leading to waste treatment

Use ISRT assays for metal content as per statistical requirements