Leaching Residue from Copper-Gold Ore Processing from Mexico

Ash-like residue from hydrometallurgical leaching of copper-gold ores, predominantly copper with embedded gold for recovery. Falls under 2620.30.00.50 for copper-main slags containing gold, used in metal extraction per heading scope. Assay reports gold content per statistical requirements.

Duty Rate — Mexico → United States

0%

Rate breakdown

9903.03.030%Articles the product of any country, as provided for in subdivision (aa)(ii) of U.S. note 2 to this subchapter

Import Tips

Submit lab assays confirming gold content and copper dominance before import

Ensure documentation proves industrial use for metal extraction to meet chapter note (a)

Avoid bulk packaging that might suggest waste disposal

Leaching Residue from Copper-Gold Ore Processing from Mexico — Import Duty Rate | HTS 2620.30.00.50