Mixed Molybdenum Flotation Concentrate

Flotation concentrate blending molybdenite and oxide minerals (e.g., wulfenite, powellite) at 45% Mo grade from polymetallic deposits. Classified as HTS 2613.90.00.00 'other' since not purely roasted molybdenite. Key input for ferroalloy production.

Import Duty Rates by Country of Origin

Origin CountryMFN RateCh.99 SurchargesTotal Effective Rate
🇨🇳ChinaFree—Free
🇲🇽MexicoFree—Free
🇨🇦CanadaFree—Free
🇩🇪GermanyFree—Free
🇯🇵JapanFree—Free

Alternative Classifications

This product could be classified differently depending on its characteristics or intended use.

2603.00.00Same rate: Free

If high copper co-product content

Copper-moly mixed concentrates classified by principal metal under 2603.

2615.90.30.00Higher: 25% vs Free

If niobium/tantalum associated

Other rare-earth/metal ores including niobium shift headings.

2620.99Higher: 10% vs Free

If from metallurgical plant residues

Slag/ash from industry for metal recovery per 2620 notes.

Not sure which classification is right?

Our AI classifier can analyze your specific product and recommend the correct HTS code with confidence.

Import Tips & Compliance

• Break down mineral composition in entry docs for customs verification of 'other' status

• Test for copper impurities; high levels may trigger 2603 classification

• Use sealed samples for disputes on metal content deductions