Kiruna Magnetite Concentrate Briquettes from Japan
High-purity LKAB Kiruna magnetite ground to <45μm, agglomerated into green pellets then hardened for DR pellet feed. Under HTS 2601.12.00 as premium agglomerated concentrate.
Duty Rate — Japan → United States
12.5%
Rate breakdown
9903.05.4912.5%Except for products described in headings 9903.05.85–9903.05.92, articles the product of Japan, with an ad valorem (or ad valorem equivalent) rate of duty under column 1 less than 12.5 percent, as provided for in U.S. note 52 to this subchapter
Import Tips
• Provide LKAB specification sheets showing 68-70% Fe content
• Ensure cold bonding strength >200 kg/pellet for transport
• Comply with REACH registration for EU-origin concentrates