</>Build with Tariff Intelligence|Programmatic access to tariff calculations and HS code classification.Explore Developer Resources →

Kiruna-Type Magnetite Pellets from Japan

High-purity pellets from Kiruna-style magnetite processing, agglomerated for electric arc furnace use. HTS 2601.12.0030 classification for agglomerated iron ore pellets.

Duty Rate — Japan → United States

12.5%

Rate breakdown

9903.05.4912.5%Section 301 (forced labor) — Japan (col1 rate < 12.5 percent): MFN < 12.5% → total duty capped at 12.5%

Import Tips

Include grind size and magnetic separation data in technical specs

Ensure no vanadium content pushes to 2614 roasted ores

Use bulk carrier manifests specifying 'pellets' to prevent lumping with fines