Beneficiated Nepheline Concentrate from Japan

Flotation beneficiated nepheline concentrate >95% purity for premium glass and ceramic applications. HTS 2529.30.0050 'other' nepheline syenite after physical separation processes. Low iron content (<0.3% Fe2O3) ensures color stability.

Duty Rate — Japan → United States

12.5%

Rate breakdown

9903.05.4912.5%Section 301 (forced labor) — Japan (col1 rate < 12.5 percent): MFN < 12.5% → total duty capped at 12.5%

Import Tips

Flotation reagent residue analysis prevents chemical preparation misclassification

Fe2O3 <0.3% certificates mandatory for glass color specifications