Molybdenum Powder for Superalloy Production
Coarse molybdenum powder used in vacuum arc remelting for nickel-based superalloys in turbine blades. It is base molybdenum powder with a 50-150 micron size range, meeting the Chapter 81 definition of powders. This product is classified under tariff item 8102.10.00 as molybdenum powder.
Import Duty Rates by Country of Origin
| Origin Country | MFN Tariff | Surtaxes | Total Effective Rate |
|---|---|---|---|
| π¨π³China | Free | β | Free |
| π²π½Mexico | Free | β | Free |
| πΊπΈUnited States | Free | β | Free |
| π©πͺGermany | Free | β | Free |
| π―π΅Japan | Free | β | Free |
PGA flags
No agency flag on this HTS number in the CBSA Single Window matching criteria.
CBSA Single Window matching criteria, unknown
Alternative Classifications
This product could be classified differently depending on its characteristics or intended use.
If the product is in a form other than powder, such as briquettes or compacts
Molybdenum articles other than powders are classified separately.
Not sure which classification is right?
The Tariff Assistant works through the GRI rules on your specific product to reach the right tariff item β and can price the duty on it in the same conversation.
Import Tips & Compliance
β’ Confirm the powder's purity (>99%) and particle size (50-150 microns) to support classification
β’ Provide end-use documentation for superalloy production to avoid scrutiny
β’ Check if the powder is subject to Canadian import restrictions for strategic materials
Related Products under Tariff item 8102.10.00
Atomized Molybdenum Powder for Thermal Spraying
Atomized molybdenum powder designed for plasma or HVOF thermal spray coatings on industrial components. It is a pure molybdenum powder (molybdenum >99% by weight) that meets the Chapter 81 definition of powders, with 90% or more passing through a 1 mm sieve. This product is classified under tariff item 8102.10.00 as molybdenum powders.
Electrolytic Molybdenum Powder
Electrolytic molybdenum powder produced by fused salt electrolysis, noted for high purity and green color. It is used primarily in lighting filament supports and other high-temperature applications. The product is a molybdenum powder with purity exceeding 99%, meeting the Chapter 81 definition of powders.
High-Purity Molybdenum Powder for Catalysts
Ultra-pure molybdenum powder used as a catalyst precursor in hydrodesulfurization processes for petroleum refining. It has a purity greater than 99.95% with controlled particle size, meeting the Chapter 81 definition of molybdenum powders. This product falls under tariff item 8102.10.00 as molybdenum powder.
Molybdenum Metal Powder 99.9% Pure
High-purity molybdenum powder with 99.9% molybdenum content, used in metallurgy and alloy production. It is explicitly covered under tariff item 8102.10.00 as molybdenum powder, meeting the Chapter 81 definition of powders. The product is unwrought and not alloyed, with purity exceeding 99%.
Molybdenum Powder for 3D Metal Printing
Fine molybdenum powder optimized for selective laser melting (SLM) in additive manufacturing of high-temperature parts. It is unwrought molybdenum powder with purity exceeding the Chapter 81 alloy threshold, making it classifiable under tariff item 8102.10.00. The powder is specifically designed for 3D metal printing applications.
Molybdenum Powder for Sintered Parts
Press-and-sinter grade molybdenum powder for manufacturing heat sinks and electrical contacts, with a uniform 5-20 micron size distribution. It is unwrought molybdenum powder meeting the Chapter 81 definition of powders, with purity exceeding 99%. This product falls under tariff item 8102.10.00 as molybdenum powder.