New

Ask Wove anything about tariffs.

Try Tariff Assistant

Inconel 625 Hot-Rolled Superalloy Steel Coil

Inconel 625 is a high-nickel superalloy steel with approximately 58% nickel, supplied as a hot-rolled coil with a thickness of 4.75 mm or more and a width of 600 mm or more. It is not further worked than hot-rolled, classifying it as a flat-rolled product of other alloy steel under tariff item 7225.30.00. This material is widely used in aerospace and chemical industries for its high-temperature strength and corrosion resistance.

Import Duty Rates by Country of Origin

Origin CountryMFN TariffSurtaxesTotal Effective Rate
🇨🇳ChinaFree—Free
🇲🇽MexicoFree—Free
🇺🇸United StatesFree+50.0%50%
🇩🇪GermanyFree—Free
🇯🇵JapanFree—Free

More Specific Codes

This product may fall under a more specific subheading:

Alternative Classifications

This product could be classified differently depending on its characteristics or intended use.

7225.40.00Same rate: Free

If the product is in straight lengths rather than coils

Flat-rolled products of other alloy steel, not further worked than hot-rolled, but not in coils.

7226.20.00Same rate: Free

If the width is less than 600 mm

Flat-rolled products of other alloy steel, of a width of less than 600 mm, not further worked than hot-rolled.

7506.20.10Same rate: Free

If the nickel content predominates and it is classified as a nickel alloy

Products of nickel alloys, in plates, sheets, strip and foil, if the material is predominantly nickel by weight.

Not sure which classification is right?

The Tariff Assistant works through the GRI rules on your specific product to reach the right tariff item — and can price the duty on it in the same conversation.

Import Tips & Compliance

• Document the nickel content (≥58%) and dimensions clearly, as CBSA may require proof that the product is not further worked than hot-rolled

• Include a certificate of analysis to confirm the alloy composition

• If the coil has been annealed or pickled, it may be classified under a different subheading

Related Products under Tariff item 7225.30.00

A2 Tool Steel Hot-Rolled Coil

A2 tool steel hot-rolled coil, 5.5 mm thick and 1000 mm wide, supplied in coils without further working. A2 is an air-hardening tool steel with high carbon and chromium content, making it an alloy steel under Chapter 72. The product is flat-rolled, of a width exceeding 600 mm, and not further worked than hot-rolled, fitting the tariff item.

AL-6XN Hot-Rolled High-Nickel Alloy Coil

This is a hot-rolled coil of AL-6XN super-austenitic high-nickel alloy steel, containing at least 24% nickel by weight, with a thickness of 4.75 mm or more and a width of 600 mm or more. It is classified under tariff item 7225.30.00 as a flat-rolled product of other alloy steel, not further worked than hot-rolled, in coils. The product has a black finish from hot rolling and is not further processed.

Alloy 20Cb-3 Hot-Rolled High-Nickel Steel Coil

This is a hot-rolled coil of Alloy 20Cb-3 (Incoloy 20), a high-nickel austenitic alloy steel containing about 35% nickel, with a thickness of 4.75 mm or more and a width of 600 mm or more. It is classified under tariff item 7225.30.00 as a flat-rolled product of other alloy steel, not further worked than hot-rolled, in coils. The product is supplied in coils without further surface treatment.

Carpenter 20 Hot-Rolled Alloy Steel Coil

This is a hot-rolled coil of Carpenter 20Cb-3 high-nickel stainless steel, with a thickness of 4.75 mm or more and a width of 600 mm or more. It is classified under tariff item 7225.30.00 as a flat-rolled product of other alloy steel, not further worked than hot-rolled, in coils. The product is supplied in coils without further processing.

CPM-10V Tool Steel Hot-Rolled Coil

CPM-10V tool steel hot-rolled coil, 10 mm thick and 1600 mm wide, for wear-resistant knives. CPM-10V is a powdered metallurgy tool steel with high carbon and vanadium content, classified as other alloy steel. The product is flat-rolled, wide, and in coils, not further worked.

CPM-M4 Tool Steel Hot-Rolled Coil

CPM-M4 tool steel hot-rolled coil, 6.5 mm thick and 950 mm wide, produced by powder metallurgy. This alloy steel contains high carbon and chromium, qualifying as tool steel. The product is flat-rolled, over 600 mm wide, and in coils, not further worked than hot-rolled.