D2 Tool Steel Die Scrap

Broken D2 tool steel dies from stamping operations, containing 1.5% carbon and 12% chromium. This material is classified under 7204.29.00 as other alloy steel waste and scrap because D2 is a high-carbon, high-chromium tool steel that is not stainless (chromium content is above 10.5% but the carbon content exceeds the stainless steel definition). It is suitable for remelting.

Import Duty Rates by Country of Origin

Origin CountryMFN TariffSurtaxesTotal Effective Rate
πŸ‡¨πŸ‡³ChinaFreeβ€”Free
πŸ‡²πŸ‡½MexicoFreeβ€”Free
πŸ‡ΊπŸ‡ΈUnited StatesFreeβ€”Free
πŸ‡©πŸ‡ͺGermanyFreeβ€”Free
πŸ‡―πŸ‡΅JapanFreeβ€”Free

More Specific Codes

This product may fall under a more specific subheading:

Alternative Classifications

This product could be classified differently depending on its characteristics or intended use.

7204.21.00Same rate: Free

If the chromium content is 10.5% or more and carbon is 1.2% or less

Stainless steel scrap is classified under a different item.

Not sure which classification is right?

The Tariff Assistant works through the GRI rules on your specific product to reach the right tariff item β€” and can price the duty on it in the same conversation.

Import Tips & Compliance

β€’ Confirm the carbon content exceeds 1.2%, which excludes it from stainless steel classification

β€’ Provide a mill certificate or analysis

β€’ Be prepared to explain why the dies are not usable as tools

Related Products under Tariff item 7204.29.00

17-4PH Stainless Alloy Scrap

Scrap from 17-4PH precipitation hardening stainless steel aerospace forgings. This material is classified as alloy steel waste and scrap under tariff item 7204.29.00 because it does not meet the definition of stainless steel (chromium content below 10.5%) or falls outside the specific stainless steel scrap subheadings. It is suitable for remelting in specialty steel production.

4340 Alloy Steel Borings Scrap

Fine borings from 4340 nickel-chromium-molybdenum steel aerospace components. These are classified as alloy steel waste and scrap under 7204.29.00 because 4340 is an alloy steel (not stainless) and the borings are not usable as finished parts. They are ideal for remelting in specialty steel production.

AISI 4140 Alloy Steel Scrap

Remelting scrap consisting of discarded AISI 4140 chromium-molybdenum alloy steel parts from machining operations. This material is classified under 7204.29.00 as waste and scrap of alloy steel, other than stainless, because 4140 contains chromium and molybdenum but does not meet the stainless steel threshold. It is suitable for remelting into new alloy steel products.

AISI 8620 Gear Blank Scrap

Unfinished gear blanks scrapped from 8620 carburizing alloy steel production. These blanks are classified under 7204.29.00 as other alloy steel waste and scrap because 8620 is a nickel-chromium-molybdenum alloy steel that is not stainless. The scrap is valuable for remelting into new gear manufacturing stock.

Ball Bearing Steel 52100 Scrap

Scrap rings and balls from 52100 alloy steel bearings. This material is classified under 7204.29.00 as other alloy steel waste and scrap because 52100 is a high-carbon chromium alloy steel that is not stainless. It is suitable for remelting into new bearing production.

Chipper Knife Steel Scrap

Worn chipper knives made from alloy tool steel with a composition of 0.48-0.55% carbon and 7.25-8.75% chromium. These are classified under 7204.29.00 as other alloy steel waste and scrap because they are not stainless (chromium below 10.5%) and are no longer usable as knives. They are suitable for remelting.